- Steel OSV1 round bar
- Steel OSV1 forging
- Steel OSV1 sheet
- Steel OSV1 flat bar
- Steel OSV1 pipe
Steel OSV1
Production specification
Square-shape steel: 1mm to 4000mm
Plate steel:0.1mm to 4000mm
Width: 10mm to 2500mm
Lenth: We can supply any lenth based on the customer's requirement.
Forging: Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes
Tubings: OD: φ6-1800mm, with wall thickness ranging from 1-35 mm.
Finished goods condition: hot forging/hot rolling + annealing/normalizing + tempering/quenching + tempering/any conditions based on the customer's requirement
Surface conditions: scaled (hot working finish)/ground/rough machining/fine machining/based on the customer's requirement
Furnaces for metallurgical processing: electrode arc + LF/VD/VOD/ESR/Vacuum consumable electrode.
Ultrasonic inspection: 100% ultrasonic inspection for any inperfections or based on the customer's requirementExcellent service for all kinds of industries,with advantages of technologies, equipment and price.
We serve you with our honesty, integrity, and professionality.
Steel OSV1 Tool Steel
Designation by Standards
Brand Name | LH No. | Mat. No. | DIN | EN | AISI |
OSV1 | 841 | - | - | - | - |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
1.53 | 0.25 | 0.25 | 4.90 | - | 5.00 | 6.50 | - | Co: 4.90 |
Description
OSV1 is medium Cr-Mo-V-W-Co high-speed steel with good wear resistance and toughness. The additional cobalt content produces a high degree of hot hardening and tempering resistance.
Applications
Sendzimir rolls, cutting tools, stamping, woodworking, drawing, deep drawing and pressing tools.
Physical properties (avarage values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 217
Density [g/cm3]: 8.2
>
Soft Annealing
Please ask.
Stress Relieving
Stress relieving to remove machining stresses should be carried out by heating to 600-650oC, holding for one hour at heat, followed by air cooling. This operation is performed to reduce distortion during heat treatment.
Hardening
Please ask.
Tempering
Tempering temperature: See the data bellow.
Tempering Temperature (oC) vs. Hardness (HRC)
100oC | 200oC | 300oC | 400oC | 450oC | 500oC | 550oC | 600oC | 650oC |
64.0 | 62.0 | 60.0 | 60.0 | 61.5 | 64.0 | 63.5 | 59.0 | 52.0 |
Forging
Hot forming temperature: 1100-900oC.
Mechanical properties
Heat treatment
Machining
Welding performance